Effect of Elemental Sulfur on Pitting Corrosion of Steels

Muthukumar Nagu*, Abdullatif Abdulhadi, Abdulrahman Huwaiji and Nayef M Alanazi

This paper focuses on studying the pitting corrosion tendency of austenitic stainless steels (SS 316 L and NIT 60) and carbon steel (API 5 LX 60) in the presence of elemental sulfur. The pitting corrosion tendency of alloys was studied by using cyclic polarization technique at two different temperatures with and without elemental sulfur. Surface morphology and corrosion products formed on the exposed coupons were analyzed by scanning electron microscopy (SEM) and energy dispersive X-ray (EDX). It was found that the temperature played major role on pitting corrosion of alloys in presence of elemental sulfur. SS 316 L gave high pitting resistance than other tested alloys (NIT 60 and API 5 LX 60).

மறுப்பு: இந்த சுருக்கமானது செயற்கை நுண்ணறிவு கருவிகளைப் பயன்படுத்தி மொழிபெயர்க்கப்பட்டது மற்றும் இன்னும் மதிப்பாய்வு செய்யப்படவில்லை அல்லது சரிபார்க்கப்படவில்லை
இந்தப் பக்கத்தைப் பகிரவும்